Polypropylene Polymer Synthetic MacroFiber For Concrete Reinforcement
Contact Person : Jack
Phone Number : 0086-13955140199
WhatsApp : +8613955140199
Minimum Order Quantity : | 1000kgs | Price : | FOB Qingdao Port,China |
---|---|---|---|
Packaging Details : | 1kg/PE film bag, 10kg/Plastic Woven bag,5500kgs/20'gp,12000KG/20'gp | Delivery Time : | Within 15days after order confirmation |
Payment Terms : | L/C, D/A, D/P, T/T, , MoneyGram | Supply Ability : | 10000TON PER YEARS |
Place of Origin: | Anhui | Brand Name: | ELITE-INDUE |
---|---|---|---|
Certification: | CE ISO | Model Number: | Elt-Twist |
Detail Information |
|||
Material: | PP | Length: | 48MM 54MM |
---|---|---|---|
Elastic Modulas: | Min 3500MPa | Equivalent Diameter: | 0.3+/-0.03mm |
Melting Point(C Deg.): | 160 - 170 | Density(g/cm3): | 0.91+/-0.01 |
Tensile Strength(MPa): | 500MPA To 800Mpa | Color: | Gray/black/white |
Use: | Concrete Reinforcement | ||
High Light: | PP Macro Structural Fiber,Hybrid Type PP Macro Fiber,Twist PP Structural Fiber |
Product Description
Polypropylene PP Macro Structural Synthetic Fiber Twist Hybrid Type 54mm
1, Description:
EltFiber-Twist can be used to instead of steel fibre for reinforcement to cement concrete.
Compared with steel fibre, it has the advantage of easy dispersing and blending, no damage to the mixing equipments, etc
ELT-TWIST is a 100% virgin blended copolymer synthetic Structural macro-fiber successfully used as an alternate to steel fibers, welded wire
mesh and conventional reinforcing bars in a wide variety of secondary reinforcement applications.
ELT-Twist is actually a Hybrid of two fibers:A standard fibrillated polypropylene fiber to reduce and control shrinkage and temperature cracking.
A twisted-bundle monofilament fiber made of a strong synthetic copolymer, to increase load-transfer and post-crack performance.
2, Production Process
3, Specification:
Density(g/cm3)
|
0.91 +/- 0.01
|
Raw material
|
PP
|
Length(mm)
|
48mm,54mm
|
Equivalent Dia(mm)
|
0.3±0.03
|
Shape
|
twist
|
break tensile Ratio(%)
|
8-15
|
Crack Ratio
|
20+/-5 %
|
Melting point ( C. Deg)
|
160-170
|
Tensile Strength
|
>500 MPa
|
Water absorbency
|
NO
|
Elastic Modulus (mPa)
|
>3500
|
Resistance to acid & alkali
|
strong
|
4, Packing:
5, Applying Instruction:
1, Ration design of the fibre concrete:
Generally the recommended amount to add to the concrete is more than 2.7kg per sqm ( volume ratio is 0.3% ),reinforcement adding
amount is 5.5kg, Compared with adding 47kg of steel fibre, 5.4kg polymer fibre has the same volume ratio to the concrete.
2, Length:
48mm or 54mm for common crack-resistant requirement. Other length can as per your request,such as 19mm
3, Matching Ratio:
Usually, it is no need to Change the matching ratio of the concrete. Considering the requirement of fissure-resistant, the polymer
fiber is recommend to combine with the polypropylene fiber mesh with the volume ratio of 1:1 ( 0.9kg fiber-mesh per sqm of cement concrete).
4, Mixer Adoption: Double-axle horizontal compelling mixer is priority.
5, Mixing process:
Crushed stones, fibers and sands are put into the mixer in succession. After stirring for two minutes,fiber will fully spread and then add
cement and water and stir normally. The addition of materials also can be put into as common concrete, but the stirring time should be
properly prolonged to make fiber completely Mixed.
6, Shaping & Maintenance
There is no special requirement, may along the vibrating time for 30s, The maintenance of the fibre concrete should be done same
as the normal concrete.
6, CERTIFICATE:
Our Mainly Product and Production Capacity as below:
Main Item
|
Capacity/Annual
|
||
Polypropylene Fiber (PP Fiber)
|
15000mts
|
||
Polyester Fiber(PET Fiber)
|
6000mts
|
||
Polyvinyl Alcohol Fiber( PVA Fiber)
|
30000mts
|
||
Polyacrylonitrile Fiber(PAN Fiber)
|
6000mts
|
||
Naphthalene Formaldehyde Sulphonate
|
300000mts
|
||
Polycarboxylate Superplasticizer(Flake/Powder/Liquid)
|
150000mts
|
||
Foam Agent
|
30000mts
|
7, Related Product:
Enter Your Message